PREVOST H3-41 Maintenance Manual page 837

Hide thumbs Also See for H3-41:
Table of Contents

Advertisement

WHEN SHOULD A STRUCTURE INSPECTION BE CARRIED OUT?
Vehicles operating in harsh environments without an appropriate corrosion protection compound applied
to the front and rear sub-frames, drive axle cradle and tag axle could be subject to corrosion. If parts of the
tag axle or front and rear sub-frames structures present metal flaking, separation of metal layers, loss of
material, perforation, etc. then they should be inspected in order to confirm that the minimum wall
thickness remains (
FIGURE 2
FIGURE 2: METAL FLAKING. ACCUMULATED SAND AS
SHOWN ON THE IMAGE SHOULD NOT BE LEFT IN PLACE
FIGURE
4:
METAL
FLAKING
ACCUMULATED MATTER WILL RETAIN WATER THUS
CREATING
CONDITIONS
CORROSION
to
).
FIGURE 5
ON
TAG
AXLE
-
PROMOTING
ADDITIONAL
FIGURE 3: METAL FLAKING AND ACCUMULATED SAND
FIGURE 5: HEAVILY CORRODED
TAG AXLE. THIS IMAGE SHOWS THE SPINDLE MOUNTING
PLATE SEPARATED FROM THE REST OF THE TAG AXLE
MI15-18 / Page 3 / 6
COACH WITH BROKEN
<QF7720955 rev 2>

Hide quick links:

Advertisement

Table of Contents
loading

This manual is also suitable for:

H3-45H3-45 vipX3-45X3-45 vip

Table of Contents