Agilent Nano Indenter G200 User's Guide
Figure E-14Optical image of a scratch made with the edge of a cube
corner
Figure E-15
shows the evolution of the pile-up height due to
visco-plastic relaxation after the scratch is made (for different systems
of automotive paints).
Figure E-15Evolution of the Pile-Up Height due to visco-plastic
relaxation
Maintaining the same normal load, variation in scratch velocity results
in a variation of the scratch width. Faster motion results in a thinner
residual scratch, corresponding to a harder material.