BO−22
Primer M
Primer M
Primer M
1996 TOYOTA T100 (RM449U)
BODY
6.
Using a brush, coat the contact surface on the body with Primer
M.
NOTICE:
Adhesive
S
S
S
N00141
7.
Primer G
(a)
(b)
NOTICE:
S
S
N06556
8.
NOTICE:
S
S
(a)
(b)
BO4422
9.
(a)
HINT:
15 mm
After cutting off the tip, use all adhesive within the time de-
(0.59 in.)
scribed in the chart below.
7 mm
(0.28 in.)
N06484
(b)
(c)
WINDSHIELD
COAT CONTACT SURFACE OF BODY WITH PRIMER
"M"
Let the primer coating dry for 3 minutes or more.
Do not coat Primer M to the adhesive.
Do not keep any of the opened Primer M for later use.
COAT CONTACT SURFACE OF GLASS WITH PRIMER
"G"
Using a brush or sponge, coat the edge of the glass and
the contact surface with Primer G.
Before the primer dries, wipe it off with a clean shop rag.
Let the primer coating dry for 3 minutes or more.
Do not keep any of the opened Primer G for later use.
MIX ADHESIVE COATING
Be sure that installation of the moulding is finished
within usable time.
The mixture should be made in 5 minutes or less.
Throughly clean the glass plate and putty spatula with sol-
vent.
Thoroughly mix 500 g (17.64 oz.) of the main agent and
75 g (2.65 oz.) of the hardening agent on a glass plate or
like object with a putty spatula.
APPLY ADHESIVE
Cut off the tip of the cartridge nozzle.
Part No. 08850−00801 or equivalent
Temperature
35°C (95 °F)
20°C (68 °F)
5°C (41 °F)
Load the cartridge into the sealer gun.
Coat the glass with adhesive, as shown.
Tackfree time
15 minutes
100 minutes
8 hours