The measurement data serves as input for the voltage control. The process reduces heat input, deformation and spatter.
WiseThin+ is also optimal for position welding with thicker plates.
>> To take WiseThin+ into use, go to AX Manager's Welding parameters view and apply WiseThin+. Optionally,
go to the Memory channels view and create a new memory channel with WiseThin+ process.
>> Adjust the wire feed speed in the Home view.
>> Fine-tune the heat output while welding in the Home view.

3.3.8 MAX Cool process

MAX Cool is a synergic MIG/MAG welding process that is designed for root pass welds and sheet metal applications.
MAX Cool is suitable for all welding positions and provides a smooth arc, reducing spatter.
>> To take MAX Cool into use, go to AX Manager's Welding parameters view and apply MAX Cool. Optionally, go
to the Memory channels view and create a new memory channel with MAX Cool process.
>> Adjust the wire feed speed in the Home view. The adjustment's effect on the plate thickness is also shown.
>> Fine-tune the heat output in the Home view.
MAX Cool supports these filler wire and shielding gas combinations:
Fe solid & Ar + 18...25 % CO
Fe solid & CO
Ss solid & Ar + 2 % CO
CuSi3 & Ar (1.0 mm)
CuAl8 & Ar (1.0 mm).

3.3.9 MAX Position process

X5 Power Source Pulse/Pulse+
MAX Position is a synergic MIG/MAG welding process optimized for vertical fillet welds (position: PF). MAX Position auto-
matically switches between two separate power levels. The two power levels can use the same welding process or two
different welding processes.
>> To take MAX Position into use, go to AX Manager's Welding parameters view and apply MAX Position. Option-
ally, go to the Memory channels view and create a new memory channel with MAX Position process.
>> In the Welding parameters view, MAX Position frequency can be adjusted and the optional WiseFusion fea-
ture can be applied. The ratio of the two power levels is preset.
>> Adjust the average wire feed speed in the Home view. The adjustment's effect on the plate thickness is also
shown.
>> Fine-tune the welding voltage in the Home view.
MAX Position supports these filler wire and shielding gas combinations:
Fe solid & Ar + 18% CO
Fe solid & Ar + 8% CO
Fe MC & Ar + 18% CO
Ss solid & Ar + 2% CO
AlMg & Ar (1.0 mm, 1.2 mm)
MAX Position supports these plate thicknesses:
3...12 mm
MAX Position utilizes also other welding processes, depending on the material and equipment type:
Fe & Fe MC: 1-MIG (with low power) and Pulse MIG (with high power)
Ss & Al: Pulse MIG (throughout the power range).
© Kemppi
(1.0 mm, 1.2 mm)
2
(1.0 mm, 1.2 mm)
2
(1.0 mm, 1.2 mm)
2
(1.0 mm, 1.2 mm)
2
(1.0 mm, 1.2 mm)
2
(1.2 mm)
2
(1.0 mm, 1.2 mm)
2
140
AX MIG Welder
Operating manual - EN
1921900 / 2318

Advertisement

Table of Contents
loading

Table of Contents