1.15 Repair methods
To repair a crack, the weld bead must be ground along the full
length of the crack to twice the depth of the crack itself before
repeating the weld (Fig. C). After welding, crack testing must
be repeated.
Cracks in the outer skin are repaired by drilling a 2 mm diameter
hole at each end of the crack to prevent it from spreading.
Then both the crack and the holes are welded (Fig. D).
Copyright ©
2010
C
Crack
Approximately double the length of the crack
D
Hole
Hole