Conducting the Tape Adhesion Test
Step
Procedure
5
If the tape test indicates inadequate adhesion, increase the heat setting by 5
degrees, print another card and try the tape test again.
•
Once the temperature has been increased 4 times (20 degrees), reset
temperature to default and increase the Dwell Time by .5 second.
•
Repeat this process until adequate adhesion is achieved.
•
Ensure that the cards (in use) have a surface roughness (Ra) of 60 micro
inches or less.
This information should be available from the card manufacturer.