1. After the part is completely dry, insert the part into your UV oven in the
same orientation it was printed in, as if the bottom of the curing oven
is the print platform. Please see the image below for reference.
CAUTION: Use nitrile gloves whenever touching
or operating the LC-3DPrint Box. Normal usage of the
oven will most likely get uncured material on the box
handle, buttons, and screen; so it is always best to take
this precaution.
 
2. Follow instructions in your UV oven instruction manual to begin the post-curing process. If you have the LC-3DPrint
Box, the instruction manual can be found both in the packaging or by downloading the link
Box Instructions for
3. Please see
the Material Stirring and Curing
open the curing chamber door until the curing process has been completed. The LC-3DPrint Box has a sensor that will
turn the machine off during curing if the lid is open. Please see the Instructions for Use of the material you are using for
full post-curing instructions.
4. Once the printed part has been fully cured, remove the part from the UV oven, using nitrile gloves when opening and
closing the oven.
5. Inspect the part for surface tackiness and/or areas of discernable liquid material. If either condition exists, clean the
part with recommended solvent once more and put it back in the UV oven until there is no more uncured material on
it. The printed part is now safe to touch without nitrile gloves.
CAUTION: Be careful not to over-cure the part. Over-curing can cause discoloration and part warping.
. You may now wish to further re ne the part's shape with ne-grit sandpaper or dental tools, removing any remnants of
supporting architecture that remain on the part.
Clean Print Platform and Print Tray
CAUTION: Do not clean the print platform or print tray in a sink or tub that drains into wastewater. These
components must be cleaned in a self-contained tub and the solvent/material mix must be discarded
according to all local, state, and federal regulations.
infocenter.3dsystems.com/fabpro1000/print/book/export/html/526
Use.
Chart for a quick reference of curing times for different materials. Do not
User Guide
here: NextDent LC-3DPrint
75/111

Advertisement

Table of Contents
loading

Table of Contents