During Submerged Arc Welding (SAW), an arc melts a continuously supplied wire. The weld
pool is protected by flux.
Aristo® 1000: When the SAW process is selected, choose METHOD with the positioning
knob and press ENTER. Choose AC or DC.
SAW
PROCESS
METHOD
REGULATION TYPE
WIRE TYPE
WIRE DIMENSION
CONFIGURATION►
TOOLS►
SET
MEASURE
Aristo® 1000: When the SAW process is selected, you can choose between three control
methods by marking REGULATION TYPE using the positioning knob and pressing ENTER.
Choose between constant welding current CA or constant wire feed CW or constant current
CC.
LAF/TAF: When the SAW process is selected, you can choose between three control
methods by marking REGULATION TYPE using the positioning knob and pressing ENTER.
Choose between constant welding current CA or constant wire feed CW.
See explanations in "CA, constant amperage", "CW, constant wire feed" and "CC, constant
current".
If ICE wire feed is selected, see  "ICE wire feed", page 53, only regulation type CW can be
selected.
3.1

Settings for submerged arc welding

Settings
1)
Arc voltage
  For Aristo® 1000
  For LAF/TAF
1)
Welding current
(CA)
1)
Wire feed speed
(CW)
1) 3)
Constant current
1)
ICE wire feed speed
1)
ICE wire start delay
Travel speed *
Welding direction
3)
AC frequency
0460 949 474
MEMORY
Setting range
14 -50 V
8 - 60 V
0 - 3200 A
0 - 2500 cm/min
0 - 3200 A
(CC)
0 - 200%
0 - 99,0 s
0 - 200 cm/min
▲-■
10 - 100 Hz
FAST MODE
In steps of
0.1 V (1V)
0.1 V (1V)
1 A
1 cm/min
1 A
1%
0,1 s
1 cm/min
-
1
- 17 -
SAW
AC
CC
Fe SOLID
0.8 mm
Value after
resetting
30 V
30 V
400 A
100 cm/min
500 A
100%
2,5 s
30 cm/min
50 Hz