2. Use sanding paper to remove protruding material.
3. Clean the area with cleaning agent and leave it dry 5 min.
4. Apply a thin layer of adhesive and leave it dry 10 min.
5. Fill the uneven surface with adhesive and smooth out with
putty knife.
6. Use an infrared light to accelerate the curing process and
raise the temperature to 60-70°C (140-158 ºF), heat 15 min.
7. Polish the dent area with sanding paper.
8. Remove dust debris.
9. Apply a thin layer of adhesive and leave it dry 10 min.
10. Restore the plastic surface according to the plastic surface
repair process.
12.11.2.4 Thermosetting Plastic Crack Repair
(length less than 100 mm)
1. Clean the area to be repaired.
2. Pry open the crack tip 5 mm (0.19 in) long, and polish it into
a V-shape crack to eliminate stress and protruding
materials.
3. Clean the area with cleaning agent and leave it dry 5 min.
4. Apply a thin layer of adhesive and leave it dry 10 min.
5. Apply
the
adhesive
part,overlapping the damaged part at least 20 mm (0.79 in).
6. Use an infrared light to accelerate the curing process and
raise the temperature to 60-70°C (140-158 ºF), heat 15 min.
7. Fill the crack area with adhesive and smooth out with putty
knife.
8. Use an infrared light to accelerate the crack tip curing
process.
9. Polish the dent area with sanding paper.
10. Apply a thin layer of adhesive and leave it dry 10 min.
11. Remove dust debris.
12. Apply a thin layer of adhesive and leave it dry 10 min.
13. Restore the plastic surface according to the plastic surface
repair process.
EC718/EC718RV EC715/EC715RV 10/2009
12-111
to
the
back
of
the
repair

Advertisement

Table of Contents
loading

This manual is also suitable for:

Ec715rv 2009Ec718rv 2009Ec715 2009

Table of Contents