Body, Sheet Metal and Painting
12.13.4.6 Plastic Surface Paint Repair Process
There are three basic requirements for the plastic surface paint
repair:
1. Paint and the plastics have a certain adhesion, without loss
of mechanical properties.
2. Paint film should have sufficient flexibility and allow the
plastic deformation without rupture.
3. Plastic pieces can reflect some of the original particles and
rough surface texture.
Plastic surface paint repair process:
Refer to the above mentioned local paint repair procedure for
plastic primer paint repair. Please note that use low
temperature baking.
Baking conditions 70-80°C (158-176 ºF),20-30 min.