130 mm
(5.2 in.)
Cause:
Due to the leading edge of the paper being curled or wavy directly after fusing, an angled force is
applied to the paper until the trailing edge of the paper moves out of the fusing unit, producing oblique
creases.
This may occur if:
• The thickness of the paper is equivalent to Paper Weight 3 or lower
• Paper smaller than A4 is used
• Printing solid fills
• Duplex printing
• To adjust the following settings, pre-register the type of paper in use as a custom paper. For details
about registering custom papers, see "Registering a Custom Paper", Paper Settings.
Solution:
1.
In [Advanced Settings] for the custom paper, increase the value in 126: [Cooling Belt
Feed Speed] by 2 percentage points.
2.
Print the image. Has the problem been resolved?
Yes
Finished!
No
Increase the speed an additional 3 percentage points in 126: [Cooling Belt Feed
Speed].
130 mm
(5.2 in.)
DFT024
Streaks
49