Pore formation
  I nadequate or missing gas shielding
Check shielding gas setting and replace shielding gas cylinder if necessary
Shield welding site with protective screens (draughts affect the welding result)
Use gas lens for aluminium applications and high-alloy steels
 Unsuitable or worn welding torch equipment
Check size of gas nozzle and replace if necessary
 Condensation (hydrogen) in the gas tube
Purge hose package with gas or replace

Bad arc ignition
 Material inclusions in the tungsten electrode due to contact with filler material or workpiece
Regrind or replace the tungsten electrode

 Bad current transfer on ignition
Check the setting on the "Tungsten electrode diameter/Ignition optimisation" rotary dial and

increase if necessary (higher ignition energy).
099-000141-EW501
12.01.2016
Rectifying faults
Checklist for rectifying faults
81

Hide quick links:

Advertisement

Table of Contents
loading
Need help?

Need help?

Do you have a question about the Tetrix 352 Synergic and is the answer not in the manual?

Subscribe to Our Youtube Channel

This manual is also suitable for:

Tetrix 452 synergicTetrix 552 synergic

Table of Contents