7. Apply mortor to the gaps left open between the island assembly (front and back).
8. Let it dry for 15 to 30 minutes and brush the area where the mortar mix was applied.
9. Prepare grout in a second container.
10. Fill the tile seam with grout using a small spatula or your finger.
11. Clean the grout with a damp rag.
12. Let the grout and mortar dry for at least three hours.

Granite Kit Instructions

Granite kits come in the following colors. Each contains various tinting colors as listed below:
Sapphire Brown
Black
White
Blue
Brown
1. Pour a small amount of epoxy and a small drop of each tint color on a piece of a cardboard.
2. Apply a small amount of the first tint color to the epoxy material using a mixing stick.
3. Mix the epoxy material well with the first tint color.
Note: Refer to the granite tint color reference chart.
4. Apply a small amount of the second tint color to the epoxy mixture.
5. Mix the epoxy mixture well with the second tint color.
6. Apply a small amount of the next tint color to the epoxy mixture.
7. Mix the epoxy mixture well with the next tint color and compare it with the color of the granite top.
8. If the colors do not match, add a tiny amount of tint color (one at a time) and mix it until you match the
color of the granite top with the epoxy mixture.
9. Once you match the color of the epoxy mixture to the color of the granite top , apply and mix a tiny amount
of hardener to the epoxy mixture.
10. Quickly fill one portion of the seam line with the epoxy mixture using a razor blade.
11. Remove the excess epoxy material from the seam line using a razor blade.
12. Let the epoxy material cure for five minutes.
13. Mark small dots in the seam line using a black permanent marker.
14. Pour a small amount of epoxy and hardener separately on a piece of cardboard.
15. Mix the epoxy material well with the hardener.
16. Quickly apply the epoxy mixture to the seam line with a razor blade.
17. Remove the excess epoxy material from the seam line using a razor blade.
18. Let the epoxy material cure for five minutes.
19. Repeat the previous steps until all the seam line is filled with epoxy mixture.
20. Clean the surface of the seam line with acetone.
Page 14
New Venetian Gold
White
Yellow
Blue
Uba Tuba (Labrador)
Black
White
Green
Giallo Veneziano
Red-Brown
Yellow
Black
White
2005 Spa Owner's Manual
7/21/2005

Advertisement

Table of Contents
loading

Table of Contents