Production Guidance; Reflow Soldering Temperature - Ebyte E104-BT02 User Manual

Table of Contents

Advertisement

Chengdu Ebyte Electronic Technology Co.,Ltd.
Poor power supply may cause messy code. Make sure that the power supply is reliable;
The extension line and feeder quality are poor or too long, so the bit error rate is high.

11 Production guidance

11.1 Reflow soldering temperature

Profile Feature
Solder Paste
Preheat Temperature min (Tsmin)
Preheat temperature max (Tsmax)
Preheat Time (Tsmin to Tsmax)(ts)
Average ramp-up rate(Tsmax to Tp)
Liquidous Temperature (TL)
Time(tL)Maintained Above(TL)
Peak temperature(Tp)
Average ramp-down rate(Tp to Tsmax)
Time 25℃ to peak temperature
Copyright ©2012–2019, Chengdu Ebyte Electronic Technology Co.,Ltd.
Profile Feature
Solder Paste
Min preheating temp
Max preheating temp
Preheating time
Average ramp-up rate
Liquid phase temp
Time below liquid phase
line
Peak temp
Average ramp-down rate
Time to peak temperature
for 25℃
E104-BT02 User Manual
Sn-Pb Assembly
Sn63/Pb37
100℃
150℃
60-120 sec
3℃/second max
183℃
60-90 sec
220-235℃
6℃/second max
6 minutes max
Pb-Free Assembly
Sn96.5/Ag3/Cu0.5
150℃
200℃
60-120 sec
3℃/second max
217℃
30-90 sec
230-250℃
6℃/second max
8 minutes max