Belts
Condition of Belt
Peeling of the belt's skin.
Wave in belt
Belt is necked down (narrow section)
Cracks or splits
One or more strands of kevlar is
hanging out, or if there is a significant
amount of frayed kevlar.
Cybex Bravo 8830/8840 Owner's Manual
3D View
Replace belt if any
section is over 1/32"
(.03) narrower than the
rest of belt
26
3D or Side View
Examine edge of belt (both sides).
Replace belt if any section is
narrower than the rest.