3.13 White spots appear at 68mm intervals
Description
Because of a soiling on the secondary transfer internal roller, white spots appeared at 68mm
intervals. When the same symptom occurs, perform the following field remedy.
Cause
A metal powder soiling existed on the surface of the secondary transfer internal roller.
Field Remedy
1. Taking care not to cause damage to the ITB belt, detach the secondary transfer internal
roller unit [A], and then clean the secondary transfer internal roller [B] with lint-free paper
moistened with alcohol.
3. Return the detached secondary transfer internal roller unit, and then make copies to
check output images.
FC5-9252 Transfer Roller2