the material inside being cured.
1. After putting the printing build plate in place, the post-processing operation of
the model is started
2. Leave trees on the surface of the model placed in the cleaning vat with alcohol
(90-95%) and soft bristle brush. The grease is cleaned off, and then the ultrasonic
cleaning printer is used for secondary cleaning
(The second cleaning time is determined by the power of the ultrasonic cleaning
printer 35w-90s. If not equipped with ultrasound cleaning machine, clean with
alcohol and soft bristle brush carefully)
Soft brush + cleaning vat
3. Place the model in a ventilated place after cleaning, or use a blower to dry the
surface alcohol of the model;
4. Place the air-dried model in a UV curing box for secondary curing.(curing time
depends on the UV used. The power of the curing box varies, 30w-240s.If not
equipped with UV curing box, the model can be placed in the sun. Let it dry for
10-15min.)
Clean up impurities in the vat
After the model post-processing is completed, the release film along the bottom
surface of the vat shall be checked for residue through the plastic scraper solid
impurities, if present, please clean up immediately. If there are many solid
ultrasonic cleaning printer