Put 5 grams (approx. one teaspoon or half a lid
full) of ANODIZING POWDER into the tray.
ATTENTION: For anodising bigger restorations
(e.g. bars, multi-unit bridges), insert twice the
amount of Anodizing Powder (two teaspoons or a
lid full) into the tray.
Stir the water well a few times until all powder has
dissolved.
Reinsert the tray into the designated fixture in the
Titanium Spectral-Colouring Anodizer.
Place the black cathode at the back, on the inside
of the tray.