2. Weld the damaged area.
• For repair of a cracked area, melt the crack together with a heat gun and a melting attachment.
• For repair of a hole, degrease the area on both sides of the bumper and apply aluminium tape on the
reverse side of the damage area.
3. Melt the polypropylene welding rod with a heat gun and deposit it the cracked area.
Note
• Heat the shaded area to melt it.
• Take care not to overlay melt welding rod. If the part is welded with the welding rod melted like jelly, the
welding strength will be reduced.
• Hold the heat gun 10—20 mm {0.39—0.79 in} from the part being welded.
• Do not move the welding rod until the welded parts cool.
VI–6
PLASTIC BODY PARTS
ZUA9818B003
ZUA9818B005
ZUA9818B004
ZUA9818B006