Download Print this page

Maintenance And Cleaning - wtw MultiLine SensoLyt 900-P Operating Manual

Ids ph electrode with polymer electrolyte

Advertisement

®
SensoLyt
900-P
Cleaning
After cleaning
ba75992e01
11/2012
11
Aging
Every pH electrode undergoes a natural aging process. With aging, the
responding behavior becomes slower and the electrode slope and asymme-
try change. Moreover, extreme operating conditions can considerably
shorten the lifetime of the electrode. These are:
 Strong acids or lyes, hydrofluoric acid, organic solvents, oils, fats, bro-
mides, sulfides, iodides, proteins
 High temperatures
 High changes in pH and temperature.
The warranty does not cover failure caused by measuring conditions and
mechanical damage.
12

Maintenance and cleaning

Remove water-soluble contamination by rinsing with deionized water. Other
types of contamination have to be removed as follows while the contact time
with the detergents should be kept as short as possible:
Contamination
Fat and oil
Lime and hydroxide deposits Rinse with citric acid (10 % by weight)
NOTE
Hydrofluoric acid, hot phosphoric acid and strong alkaline solutions
destroy the glass membrane.
Rinse the electrode with deionized water and condition it in reference elec-
trolyte solution for at least 1 hour. Then recalibrate the electrode.
Cleaning procedure
Rinse with water containing household wash-
ing-up liquid
Aging
17

Advertisement

loading