HEATING – STAGE 2
Ambient temperature settles around
set point
Internal air temperature scatter
reduces as material starts to
lay down and stick to the mold.
Curve slope flattens as powder melts
due to need to overcome latent heat
of melting.
Once powder is fully melted,
temperature rises more rapidly.
55