Post-Printing Treatment for Models Made with VeroClear

Models made with VeroClear (RGD810) have a slight yellow tint when 
removed from the printer. This is especially true for models printed with a 
glossy finish. The yellow tint fades naturally over time, but you can greatly 
accelerate this process by using a suitable photobleaching treatment.
As a rule, best clarity is achieved when parts are printed with a matte finish, 
and treated as explained below.
Photobleaching models involves exposing them to light. To achieve highly 
controlled and predictable results, a professional illumination chamber is 
recommended. However, adequate results may be obtained using ordinary 
desk lamps fitted with suitable fluorescent elements.
Figure 7-2     Left: Illumination chamber; Right: Desk lamps
 
Photo-
Follow these instructions for photobleaching printed models.
Bleaching
• The fluorescent lamps should be rated 45W, 6500K.
Instructions
• When using desk lamps, place the models in a container lined with 
• Arrange the models with enough space between them to allow light to 
• Verify that the ambient temperature around the models is approximately 
• Inspect the models after six hours of treatment. 
More information about this treatment is available in the application note 
VeroClear RGD810 Model Material.
DOC-37004 Rev. E
aluminum foil. Use at least two lamps, more when treating models in a 
large container.
reach all sides of each model.
40°C (104°F). Higher temperatures may cause model distortion; lower 
temperatures may not produce satisfactory results. When using desk 
lamps, you can achieve the required temperature by positioning the lamps 
approximately 10 cm (4 in.) above the models.
❒  For parts with a matte finish, this should be enough. Polish and 
lacquer the parts.
❒  For parts with a glossy finish, continue the photobleaching treatment 
for up to 18 hours more.
In Stratasys laboratories, there was a tint reduction of approximately 70% 