Troubleshooting - Waviness Of Bead; Troubleshooting - Distortion - Miller Electric OM-1313 Owner's Manual

Arc welding power source and wire feeder
Table of Contents

Advertisement

6-14. Troubleshooting – Waviness Of Bead
Possible Causes
Welding wire extends too far out of nozzle.
Unsteady hand.
6-15. Troubleshooting – Distortion
Possible Causes
Excessive heat input.
OM-1313 Page 28
Waviness Of Bead – weld metal that is not parallel and does not cover
joint formed by base metal.
Be sure welding wire extends not more than 1/2 in (13 mm) beyond nozzle.
Support hand on solid surface or use two hands.
Distortion – contraction of weld metal during welding that forces
base metal to move.
Base metal moves
in the direction of
the weld bead.
Use restraint (clamp) to hold base metal in position.
Make tack welds along joint before starting welding operation.
Select lower voltage range and/or reduce wire feed speed.
Increase travel speed.
Weld in small segments and allow cooling between welds.
Corrective Actions
Corrective Actions
S-0641
S-0642

Hide quick links:

Advertisement

Table of Contents
loading

This manual is also suitable for:

Millermatic 185M-15

Table of Contents