4

Chemical Resistance

4.1 Metal Casing

The frame and casing material is powder-coated aluminum. This powder paint
withstands exposure of up to 24 hours duration to the following chemicals without
visible change:
Ammonia 25%
De-ionized water
Butanol
Citric acid 10%
Diesel
Ethanol 99.5% denaturated
FAM-Normal petrol
Alcohol 95%
Phosphoric acid 43%
Glycol
Industrial petrol

4.2 Touch Screen and Overlay

4.2.1 Autotex F250

Autotex F250 covers the overlay surrounding the touch screen.
Solvent Resistance
Autotex F250 withstands exposure of more than 24 hours duration under DIN 42
115 Part 2 to the following chemicals without visible change:
Potassium ferrocyanide/
ferricyanide
Cyclohexanol
Diacetone alcohol
Glycol
Isopropanol
Glycerine
Methanol
Triacetin
Dowanol DRM/PM
Acetone
Metyl ethyl ketone
Dioxan
Cyclohexanone
Ethanol
Isophorone
Mitsubishi Electric, MA00777A
Isopropyl alcohol
Tap water
Cooling liquid 50%
Ligroin
Cooking oil
Lactic acid 10%
Sodium di-chromate
saturated
Caustic soda 5%
Sodium hypochlorite
solution
Sodium carbonate 10%
Sodium chloride 20%
Sodium hypchlorite <20%
(bleach)
Acetaldehyde
Aliphatic hydrocarbons
Toluene
Xylene
White spirit
Fromic acid <50%
Acetic acid <50%
Phosphoric acid <30%
Hydrochloric acid <36%
Nitric acid <10%
Trichloracetic acid <50%
Sulphuric acid <10%
Formaldehyde 37% - 42%
Potassium hydroxide <30%
Chemical Resistance
Nitric acid 3%
Chlorhydric acid 10%
Washer fluid 33%
Sulphuric acid 20%
Turpentine
Urea saturated
Hydroperoxide 3%
Acetic acid 10%
Alu-cleaner
-
-
1.1.1. Trichloroethane
(Genklene)
Ethylacetate
Diethyl ether
N-Butyl acetate
Amylacetate
Butycellosolve
Ether
MIBK
Cutting oil
Potassium carbonate
Washing powders
Fabric conditioner
Ferric chloride
Ferrous chlorid
Dibutyl Phthalate
4-1