6 6 . . P P o o s s s s i i b b l l e e f f a a u u l l t t s s a a n n d d t t r r o o u u b b l l e e s s h h o o o o t t i i n n g g
The power levels were set too low.
The power levels are directly related to the
calculated gold electrolyte volume.
Make a note of the correct power level for each
part, in order to set them correctly before the
process commences. (see deposition data).
see Section 9.
A power failure occurred during the electro-
forming process.
see Sections 2 and 3 (error codes)
An excess of contact adhesive has formed an
insulating layer on the copper rod.
Use a scalpel to clean the copper rod all
the way to the plaster die before applying the
conductive silver varnish.
There are gaps in the surface of the crown coping.
The surface to be electroformed was not
properly coated with conductive silver varnish
see Section 2.
The part was in contact with the beaker.
Ensure that there is always an adequate
gap between the plaster die and the beaker.
The plaster dies have fallen off.
Either too little or the wrong contact adhesive
was used, or the contact holes were too big.
Ensure that the plaster die is securely fixed
to the copper rod.
The conductive silver varnish was not applied to
the section between the plaster die and the
copper rod, and the copper rod is corroded.
Ensure that approx. 1 cm of conductive
silver varnish is applied to the copper rod and
that the shrink-fit tubing is applied at a distance
of max. 1 mm from the plaster die.
If the faults cannot be rectified with the aid of these
instructions, please contact WIELAND EDELMETALLE or
your authorized dealer.
24

Advertisement

loading

Related Products for Wieland AGC Micro Plus