Page 2
The oxide film of 10μm can affect the test result by up to 0.5~1HW. The painting on the workpiece must be removed before testing. Slow force application will result in a slightly lower reading. Use the calibration sheath with the ISHW-L20A tester when testing on thin workpiece and test block.
Page 3
Note: Do not calibrate the readings of the test block by regulating the adjustment screw. Technical specification Changing the indenter Code ISHW-L20 ISHW-L20A ISHW-L20B for aluminum for aluminum alloy for aluminum In case the reading can not be set to the full scale of 20 by regulating...
Page 4
Indenters mode point for the tester. Before calibration of the ISHW-L20A, put the calibrating sheath on the anvil first. The Webster hardness tester have different mode of indenters.