time, to purge air from the torch hose, the output of
the machine is turned ON. At this time the arc is
started according to the selected welding mode.
After the arc is started the output current will be at
the Start current. This condition can be maintained
as long or as short as necessary.
If the Start current is not necessary, do not hold the
TIG torch trigger as described at the beginning of
this step. In this condition, the machine will pass
from Step 1 to Step 2 when the arc is started.
2.
Releasing the TIG torch trigger starts the upslope
function. The output current will be increased at a
controlled rate, or upslope time, until the Welding
current is reached.
3.
Press and hold the TIG torch trigger when the main
part of the weld is complete. The machine will now
decrease the output current at a controlled rate, or
downslope time, until the Crater current is reached.
This Crater current can be maintained as long or as
short as necessary.
This sequence has an automatic restart so welding
will continue after this step. This operation, 4-step
restart enabled, is the default setting from the
factory. If the weld is completely finished, use the
following sequence instead of step 3 described
above.
3A.
Quickly press and release the TIG torch
trigger. The machine will now decrease the
output current at a controlled rate, or downslope
time, until the Crater current is reached and the
output of the machine is turned OFF. After the
arc is turned OFF the postflow time will start.
4.
Release the TIG torch trigger. The output current
will again increase to the Welding current, like in
step 2, to continue welding. When the main part of
the weld is complete go to step 3.
As shown here, after the
TIG torch trigger is quickly
pressed and released from
step 3A, it is possible to
press and hold the TIG torch
trigger another time to end
the downslope time and
maintain the output current
at the Crater current. When
the TIG torch trigger is
released the output will
again increase to the
Welding current, like in step
4, to continue welding. When the main part of the weld
is complete go to step 3.
English
As shown here, again after
the TIG torch trigger is
quickly pressed and
released from step 3A, it is
possible to quickly press
and release the TIG torch
trigger a second time to
end the downslope time
and stop welding.
04/03
Maintenance
For any maintenance or repair operations it is
recommended to contact the nearest technical service
center or Lincoln Electric.
performed by unauthorized service centers or personnel
will null and void the manufacturers warranty.
The frequency of the maintenance operations may vary
in accordance with the working environment. Any
noticeable damage should be reported immediately.
Check cables and connections integrity. Replace, if
necessary.
Keep clean the machine. Use a soft dry cloth to
clean the external case, especially the airflow inlet /
outlet louvers.
Do not open this machine and do not introduce anything
into its openings. Power supply must be disconnected
from the machine before each maintenance and service.
After each repair, perform proper tests to ensure safety.
6
WARNING
Maintenance or repairs
WARNING
English

Advertisement

Table of Contents
loading