IMPORTANT INFORMATION ABOUT LEAD FREE, (PbF), SOLDERING
If lead free solder was used in the manufacture of this product the printed circuit boards will be marked 
PbF.
Standard leaded, (Pb), solder can be used as usual on boards without the PbF mark.
When this mark does appear please read and follow the special instructions described in this manual 
on the use of PbF and how it might be permissible to use Pb solder during service and repair work.
1. ABOUT LEAD FREE SOLDER (PbF: Pb free)
Note:
In the information below, Pb, the symbol for lead in the periodic table of elements, will refer to standard 
solder or solder that contains lead.
We will use PbF when discussing the lead free solder used in our manufacturing process which is made 
from Tin, (Sn), Silver, (Ag), and Copper, (Cu).
This model, and others like it, manufactured using lead free solder will have PbF stamped on the PCB. 
For service and repair work we suggest using the same type of solder although, with some precautions, 
standard Pb solder can also be used.
Caution
- PbF solder has a melting point that is 50° ~ 70° F, (30° ~ 40°C) higher 
than Pb solder. Please use a soldering iron with temperature control 
and adjust it to 700° ± 20° F, (370° ± 10°C). In case of using high 
temperature soldering iron, please be careful not to heat too long.
- PbF solder will tend to splash if it is heated much higher than its melting 
point, approximately 1100°F, (600°C).
- If you must use Pb solder on a PCB manufactured using PbF solder, 
remove as much of the original PbF solder as possible and be sure that 
any remaining is melted prior to applying the Pb solder.
- When applying PbF solder to double layered boards, please check the 
component side for excess which may flow onto the opposite side (See 
figure, below).
1.1. SUGGESTED PbF SOLDER
There are several types of PbF solder available commercially. While this product is manufactured using 
Tin, Silver, and Copper,