Download Print this page

Amber Vest User Manual

Phosphate bound investment for casting press ceramics with normal or quick heating

Advertisement

Quick Links

Vest
User's Manual
CASTING TEMPERATURE: 850°C
250 ℃
Maintain the cylinder at the final temperature for:
CYLINDER SIZE
1 x
3x
STORAGE AND EXPIRY
Amber Vest POWDER
Store at 18-25°C.
Keep the packages tightly closed in a dry place.
The investment is sensitive to moisture: prolonged exposure to the air may alter the
characteristics of the product.
EXPANSOR-B LIQUID
35 ℃
Store at 18-25°C.
MAX.
Prolonged exposure to temperatures lower than 5°C or higher than 35°C may produce freezing
and/or destabilisation of the product.
5 ℃
Do not use the liquid if it shows a sign of cristallization.
MIN.
Keep the bottles tightly closed after each use. Prolonged exposure to the air may cause crystallisation.
Batch number and expiry date are marked on each package.
SAFETY INSTRUCTIONS
This material contains silica. DO NOT INHALE THE POWDER! Continued inhalation of the powder
may cause lung injury (silicosis or cancer).
During handling, avoid the formation of powder. Avoid inhalation by using a suitable dust mask.
Eliminate any spillages of powder with a damp cloth.
Avoid the formation of powder during deflasking by submerging the cylinder completely cold in
water. Extract the ammoniac vapours from preheating and emit them to the exterior.
Avoid skin contact with the mixing liquid EXPANSOR. In the event of contact, wash with soap
and water. In the event of contact with the eyes, wash under abundant running cold water and
consult a doctor.
Manufacturer :
Polígono Empordà Internacional 17469 VILAMALLA, GIRONA • SPAIN
Tel.: ( 34 ) 972 52 61 69 / Fax: ( 34 ) 972 52 55 86
protechno@protechno.com / www.protechno.com
850 ℃
25" / 35"
40"
After the casting has been
HEATING TIME
completed, bench-cool the ring
25 min
to room temperature.
35 min
Do not quench in cold water!!
Distributor :
77-14, Gwahakdanji-ro, Gangneung-si, Gangwon-do, KOREA 25452
Tel: 070-7712-1300 / Fax: 033-644-1231
Customer Support: 02-2083-1367 / www.hassbio.com
Phosphate bound investment for casting press ceramics
with normal or quick heating
1506EN_170711
Vest
User's Manual

Advertisement

loading
Need help?

Need help?

Do you have a question about the Vest and is the answer not in the manual?

Questions and answers

Summary of Contents for Amber Vest

  • Page 1 Do not quench in cold water!! Phosphate bound investment for casting press ceramics STORAGE AND EXPIRY with normal or quick heating Amber Vest POWDER Store at 18-25°C. Keep the packages tightly closed in a dry place. User’s Manual The investment is sensitive to moisture: prolonged exposure to the air may alter the characteristics of the product.
  • Page 2 4. MIXING Amber ® Vest is an ultra fine, graphite-free, phosphate bound investment for casting press ceramics with • Prepare the mixing liquid (EXPANSOR-B + distilled water). the technique of NORMAL OR QUICK HEATING. • Add the powder to the liquid and mix briskly by hand for 15-20 seconds to obtain According to ISO 15912:2006, the classification of the product is Type 1 Class 2.