7-13. Troubleshooting − Burn-Through
Possible Causes
Excessive heat input.
7-14. Troubleshooting − Waviness Of Bead
Possible Causes
Welding wire extends too far out of nozzle. Be sure welding wire extends not more than 1/2 in (13 mm) beyond nozzle.
Unsteady hand.
7-15. Troubleshooting − Distortion
Possible Causes
Excessive heat input.
Burn-Through − weld metal melting completely through base metal
resulting in holes where no metal remains.
Select lower voltage range and reduce wire feed speed.
Increase and/or maintain steady travel speed.
Waviness Of Bead − weld metal that is not parallel and does not cover
joint formed by base metal.
Support hand on solid surface or use two hands.
Distortion − contraction of weld metal during welding that forces
base metal to move.
Base metal moves
in the direction of
the weld bead.
Use restraint (clamp) to hold base metal in position.
Make tack welds along joint before starting welding operation.
Select lower voltage range and/or reduce wire feed speed.
Increase travel speed.
Weld in small segments and allow cooling between welds.
Corrective Actions
Corrective Actions
Corrective Actions
S-0640
S-0641
S-0642
OM-210 089 Page 35

Hide quick links:

Advertisement

Table of Contents
loading

This manual is also suitable for:

Ga16c2Mw175Ga16c2 gun

Table of Contents