TROUBLESHOOTING
• The weld did not penetrate to the rear panel.
° If using the MIG135 make sure a hole is drilled or punched in the top panel.
° Turn up the Volt setting. If this causes the wire to burn back before hitting the panel,
increase the wire speed also.
° Make sure the metal is clean. The use of a fl ap disc on all surfaces in contact and being
welded is highly recommended.
• The weld bead is too high.
° Decrease the weld time.
° Decrease the wire speed.
• The weld bead is too large in diameter.
° Decrease time of welding. Be sure not the decrease the time too much which could cause
poor penetration.