Page 2
• Variable temperatures in 10°F increments from ambient temperature to 1,200° F. • Dial-in airflow from 4 CFM to 18 CFM. • Control system prevents overheating when using specialty attachments. • Temperature & airflow lock-in feature. MASTER WELDING TIPS AND ATTACHMENTS 35017 35269 35271 1 1/4”...
Page 3
For lap welding PVC terials, such as PE, PVC, or For lap welding, Sheeting Vinyl tarpaulin. Use with 3/8” edging tape and reducer. roofing applications MASTER WELD RODS 35297 35298 35299 ABS Welding Rod PP Welding Rod PVC Welding Rod (Pkg. of 16) (Pkg.
Page 4
• Pressure. Pressure is applied by pushing down on the welding rod while weld- ing or, if butt welding, on the two edges that are being welded together. Master Appliance Corp. manufactures precise welding tips that help the welder apply equal pressure throughout the welding process.
Page 5
Break the edges of the parts to create a V-shaped groove to provide space for weld fill. Install the appropriate welding tip onto your Master Proheat heat ®...
Page 6
At the end of the weld joint cut the rod off with knife or side cutter. Allow the weld joint to cool to room temperature before testing the strength of weld. Depending on the thickness of the rod and/or the base material, more than one pass may be necessary.
Page 7
Pendulum Weld: Freehand welding. Slowly rotate the nozzle of the 3/8” reducer (35294) back and forth be- tween the workpiece and the weld rod in a pendulum motion, while applying a slight, downward force on the weld rod. Heat both the rod and the work- piece evenly.
Page 8
After cooling, the fiber-flex can be sanded with progressively finer grit until the desired surface finish is achieved. Master Appliance Corp. Phone / Téléphone / Teléfono: 2420 18th Street...